Specifications
Metal specifications for our ferritic / pearlitic S.G iron, and our certificates.

Metal specifications
SG 42
- Description
- Ferritic / pearlitic S.G iron for castings with sections thicker than 3mm.
Relevant standards
- BS2789 Grade 420/12
- SABS 936 Grade SG 42
- ASTM A536 Grade 65-45-12
- DIN 1693 Grade GGG40
- Meehanite SF 420-12
Main elements, acceptance range (%)
Carbon3,7 – 3,90
Silicon2,6 – 2,7
| Composition | Min % | Max % |
|---|---|---|
| Carbon | 3,7 | 3,90 |
| Silicon | 2,6 | 2,7 |
| Manganese | – | < 0,30 |
| Sulphur | – | < 0,02 |
| Phosphorus | – | < 0,02 |
| Nickel | – | – |
| Chromium | – | 0,10 |
| Molybdenum | – | – |
| Vanadium | – | – |
| Copper | – | – |
| Magnesium | 0,020 | 0,050 |
| Ductile iron | Tensile strength MPa (min) | % Elongation (min) | Brinell hardness (BHN) |
|---|---|---|---|
| SG 42 | 410 | 12 | < 200 max |
- Prepared by
- P. Singh
- Assisted by
- H. Joubert
- Controlled by
- A. Mwelase
- Revision
- Rev 1
- Effective date
- 01/02/2013
Certificates
Certificates
B-BBEE Level 4 contributor
West Rand Engineering (Pty) Ltd · Renaissance SA Ratings
Verification certificate
Download PDFContact
Talk to the foundry
Long production runs or shorter, lower volume orders: tell us what you need cast.